Abstract
Galvanic corrosion between 6061Al matrix and reinforcements such as graphite, SiC and Al_2O_3 phases has been studied in the deaerated, the open to air and the aerated 0.1N NaCl solutions. Based on the mixed-potential theory, the galvanic currents were measured by using the zero-resistance ammeter and the potentiodynamic polarization curves between 6061Al and reinforcements. Experimental results showed that the galvanic current densities of 6061Al-graphite couple were much higher values than those of 6061Al-SiC and 6061Al-Al_2O_3 couples. As the dissolved oxygen concentration and the surface ratio of reinforcements/6061Al matrix increased, the galvanic current densities were observed to increase.
Key Words
Galvanic corrosion, Metal matrix composites, Reinforcement, Mixed-potential theory, Zero-resistance ammeter
| PDF
대한금속∙재료학회 (06633) 서울시 서초구 서초대로 56길 38 대한금속∙재료학회 회관 (서초1동 1666-12번지)
Tel : 070-4266-1646 FAX : 02-557-1080 E-mail : metal@kim.or.kr
Copyright ⓒ 2013 사단법인 대한금속∙재료학회 All rights reserved.