A Study on the Development of oriented 3 % Silicon Steel
원동연D . Y . Won, 이희균H . K . Lee, 임호빈H . B . Im, 김정태J . T . Kim, 이건K . Lee, 김철우C . W . Kim
Abstract
A study on the development of boron 3% silicon-iron containing 0.03/0.04 C, 0.07/0.08 Mn and boron (30 ppm add) was carried out. Samples prepared by two stage cold reduction method developed complete secondary recrystallization, while samples prepared by one stage cold reduction method showed incomplete secondary recrystallization and poor magnetic properties. The magnetic properties also varied with normalizing temperature, and the sample prepared by normalizing at 950℃ showed the best magnetic properties. The induction with a magnetizing force of 800 A/m was 1.86 tesla.