Effects of Carbon Content on the Secondary Recrystallization in 3 % Si Magnetic Steel
송재성Jae Sung Song, 김영길Young Gil Kim, 임호빈Ho Bin Im
Abstract
The effects of varying carbon content (0.004∼0.098 w/o) on the secondary recrystallization in 3% Si-Fe were studied. It was found that carbon had no great influence on the cold rolled texture behavior. However, increased carbon content enhanced the development of (110) texture during primary recrystallization. When carbon content was low (0.004 w/o), poor secondary recrystallization occurred. Complete secondary recrystallization developed when carbon content was high (0.074 and 0.098 w/o).